For more information, please feel free to contact us. We are ready to answer your questions and help you further.
<p><strong>Outstanding tensile strength and flexibility:</strong></p> <p><br />* Tensile strength of 10.4 MPa – Surpassing alternatives; ensures robust and durable end</p> <p> products.<br />* Elongation at break of 346% – Maximum flexibility and stretchability for applications requiring</p> <p> the highest material mobility.</p> <p><br /><strong>Superior tear and abrasion resistance:</strong></p> <p><br />* Tear resistance of 9 N/mm – Significantly higher tear strength than reference products,</p> <p> making it ideal for highly stressed rubber products.<br />* Optimized abrasion resistance – Provides longer lifespan and stability under mechanical load.</p> <p> </p> <p><strong>Optimized electrical insulation properties:</strong></p> <p><br />* Surface resistance of 5.8 x 10⁶ Ω and volume resistance of 3.7 x 10⁶ Ω·cm – Perfect for</p> <p> applications that require high electrical insulation.</p> <p> </p> <p><strong>Efficient and controlled vulcanization:</strong></p> <p><br />* Longer vulcanization time (t90 of 14.6 minutes) – Ensures controlled, uniform crosslinking, ideal</p> <p> for homogeneous and stable structures in the final product.<br />* Lower hardness (MH of 30.4 dNm) – More flexibility in processing, enhancing the material's</p> <p> adaptability.</p> <p> </p> <p><strong>Optimal particle size distribution for even dispersion:</strong></p> <p><br />* Narrow distribution in the upper range (x90 of 6.4 µm and x99 of 11 µm) – Ensures uniform</p> <p> dispersion, better processability, and smooth surface quality in the final product.</p> <p> </p> <p><strong>Highly durable mineral composition:</strong></p> <p><br />* High content of free silica (approx. 65%) and kaolinite – Provides excellent chemical and thermal</p> <p> stability, along with superior acid resistance.</p>